當前位置:首頁技術文章不同操作條件下氧化鋁燒結對致密化的影響

不同操作條件下氧化鋁燒結對致密化的影響

更新時間:2016-07-15點擊次數(shù):3150

Nearly pure -alumina samples produced by uniaxial pressing were flash sintered under electrical fieldsranging from 500 V/cm to 1500 V/cm in experiments at constant heating rate. Sintering temperature sig-nificantly decreased with the applied E-field even down to ≈900?C at 1500 V/cm. The onset temperaturefor flash sintering can be successfully modelled as a function of the applied voltage. The sintering temper-ature is also shown to be strongly affected by the electrode materials used during the treatment: usingsilver or carbon electrodes the sintering temperature is about 300?C lower than when using platinumelectrodes. In addition, the bulk density and porosity of the sintered alumina ceramic correlate stronglywith the imposed current limit. Power dissipation was analysed before and during flash sintering; theactivation energy for conduction was calculated in both cases, indicating that the process is based onionic diffusion phenomena. Finally, we showed that during flash sintering the activation energy for con-duction decreases, suggesting the occurrence of physical or structural modifications induced by currentlocalization at the grain boundaries.

上一個:塞貝克系數(shù)測定儀的主要構成分析

返回列表

下一個:鋁酸鍶的電性能和熱膨脹系數(shù)

  • 企業(yè)名稱:

    林賽斯(上海)科學儀器有限公司

  • 公司地址:

    上海市浦東新區(qū)陸家嘴數(shù)智天地·智慧谷T3棟120號

  • 企業(yè)郵箱:

    links@linseis.com.cn

  • 聯(lián)系電話:

    021-50550642

微信公眾號

Copyright © 2025林賽斯(上海)科學儀器有限公司 All Rights Reserved  滬ICP備18045390號-2